    A friend of mine gave me several lead ingots of unkown origin. The ingots are 1 1/2 x 2 1/2 x 5 1/2 inches and weigh 6 1/2 lbs each. On the top the letters "P.L.P. CO" are visable. My friend, who is in his 60s, said these had belonged to his father, who was an electrician. He has no idea what intended use was. I don't have a hardness tester, so I can't provide Brinnell numbers. Anyone have any idea what alloy I have here?
    Attached Thumbnails Attached Thumbnails lead.jpg  

  2. #2
    Boolit Buddy
    Join Date
    Mar 2005
    Location
    Washington State
    Posts
    411

    Question Solder?

    That seems light for lead, at least fairly pure lead. I'd guess it's at least 50% tin. Prolly 50-50 solder, maybe 60 -40, or even silver solder. Other than those guesses, I dunno. Pilgrim

  3. #3
    44woody
    Guest

    lead

    if you want to melt down just enough to make 5 bullit and send it to me I will have a friend of mine test it for you give me a pm if you want to do it 44Woody
    Last edited by 44woody; 05-31-2006 at 09:39 AM.

  4. #4
    Boolit Master
    Join Date
    Mar 2005
    Location
    Trinity, Tx
    Posts
    955
    Electricians soldered joints with gimbaled solder pots well into the '60's, they were still having to do it with solder rather than crimp sleeves or wire nuts in a few cities when I started as an apprentice in '62.
    It is likely 60-40, as that was the preferred alloy for electrical use.

  5. #5
    Cast Hunter

    RugerFan's Avatar
    Join Date
    Mar 2005
    Location
    East GA
    Posts
    2,130
    It does seem fairly hard, so 60/40 sounds like a winner. Thanks for the input fellas.

    44Woody - I may get back to you later about hardness testing. - Thanks

  6. #6
    Boolit Buddy Underclocked's Avatar
    Join Date
    Mar 2006
    Location
    S.W. Missouri
    Posts
    428
    Preformed Line Products Company makes a myriad of products for the electrical and communications industries. They have locations and facilities all over the world and I'm betting your ingots have been one of their products but can find only aluminum ingots in their currect products.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check