I came across around 70 ingots of “lead” that I got from a guy who made fishing weights. He says they contain mostly lead, solder, and tin. I did pencil hardness test and Lee hardness die test and they come out around bhn 10-12. My question is, would it be acceptable to mix 50/50 with Linotype and treat it as Lyman #2? Of course I will test hardness once it’s mixed. The alloy appears very clean.